Hkust 3D Prints a Titanium Alloy That Keeps Hardening

(3dprinting.com)

51 points | by rbanffy 4 days ago ago

16 comments

  • quaffcode a day ago ago

    This is incredible. They blasted 3d waves of alloy through the metal to give different regions different, synergestic properties. And they can adjust those waves to give components different properties at specific locations. The 3d alloying waves itself seems like it could open all kinds of doors. Epic material science win.

    • bloopernova a day ago ago

      (not serious comment)

      Does this mean I can have the perfect sword, the ultimate balance of strength and flexibility?

      I'll finally be able to one-up that Scotsman with the folded steel katana made by a genius centuries ahead of his time! Or I can shut up that guy who talks my ear off about his oh so amazing Green Destiny sword.

      • adrian_b a day ago ago

        No titanium alloy is likely to be as good for swords as the best alloys based on iron, cobalt or nickel.

        Nonetheless, it might become possible to use similar methods (i.e. combining by 3D printing several different alloy powders) to create such a heterogeneous chemical composition also in some steels, and in a cheaper way than with the traditional methods of forging together different kinds of steel.

        • tosapple a day ago ago

          maybe turbines? propellers and sword design rely partially on mass/weight.

  • kavalg a day ago ago

    It would be great if someone clarifies the practical implications. For example, are we going to get better tooth implants? Are we going to create micro robots in space etc.?

    • adrian_b a day ago ago

      For tooth implants, the best material is commercially pure titanium (which contains only very small amounts of iron and oxygen impurities).

      CP titanium has enough strength for tooth implants and it has the best chemical resistance to corrosion and the least probability of introducing in your body any harmful substances.

      Alloys like Ti-Al-V should never be used for body implants, because they can leak toxic ions, though unscrupulous surgeons use such alloys, because they are much cheaper, being used in great quantities in the aerospace industry, than titanium alloys developed specially for medical implants, which contain less toxic metals, but which are more expensive.

      While CP titanium is the best for tooth implants, for some other skeleton implants stronger alloys may be needed, but those should not use vanadium, but safer metals, like niobium, molybdenum and iron. It is better if they also do not contain aluminum.

      Such a technique, of mixing during 3D printing several distinct kinds of metallic alloy powders, should be applicable also for other alloys than those from TFA, but obviously more research is needed to find suitable combinations, where useful mechanical properties are obtained.

  • lp92 2 days ago ago

    Doesn't titanium naturally age harden?

    • metal_am a day ago ago

      No. Aluminum does though

      • adrian_b a day ago ago

        Not pure aluminum, but many aluminum alloys, e.g. duralumin, which is the first metallic alloy where this phenomenon has been discovered.

        In general, age hardening is something that can happen only in alloys, not in pure metals, though there are metals, like titanium, where extremely small amounts of impurities can have great effects, so compositions that would be considered pure enough for other metals behave like alloys, by having mechanical properties very different from the really pure metal.

        The so-called "commercially-pure" titanium, in which no intentional alloying elements are added, behaves like a series of titanium alloys with small amounts of iron and oxygen, in which a great range of mechanical properties can be obtained.

      • HWR_14 a day ago ago

        Does it get more brittle or otherwise have a negative property associated with age? And does Titanium avoid that because it doesn't age harden?

        • metal_am a day ago ago

          So, lots of things going on here. Natural aging is age hardening at room temperature. Everything in engineering is a tradeoff, so you do lose a little ductility as it gets stronger, but I wouldn't call aluminum in this context brittle.

          Some Ti alloys can be age hardened. It's just not going to happen while it's sitting at your desk.

        • anjel a day ago ago

          My data is older but it used to be Ti bike frames had to dis and re-assembled periodically or, over time, Ti on Ti surfaces would self-weld (no heat req'd)

  • metalman a day ago ago

    this is a very significant development that applys known materials science properties in ways that are difficult to achive useing other methods, interestingly it uses molybdenum concentrations in a simmilar way as wootz steel (true damascuss), but in an easier to mass produce manner, but by easier I mean ferosiously difficult, unless you have essentialy perfect control of the purity of your ingredients,low parts per million or less, parts per 10 million. this is also going to remain stupidly expensive, but for certain parts , in things like turbines and pump housings that can be subject to tremendous forces, vibration, and differtial heating, and ablative wear, plus things like cavitation shock waves, or worse :) The 12% ductility is huge, and opens up other possible manufacturing steps to what are otherwise very dificult to work with alloys. First thing to clear up will be if there is internal corrosion, unlikely, but how it behaves at high temperature and vibration with possible electrical fields will need to be understood, as this will be an exotic material for exotic conditions.

  • RZhang777 a day ago ago

    Turning compositional heterogeneity in LPBF from a defect you try to anneal away into a deliberate design lever is a really clever angle.

    From a manufacturing and qualification standpoint, I'm curious how repeatable those microscale Mo waves are across different powder lots and multi-laser builds. Aerospace and medical buyers usually rely on uniform chemistry specs for NDT and lot certification, so qualifying a deliberately heterogeneous microstructure seems like a big hurdle on its own.

    Also wondering what a 557 MPa strain-hardening increment does to post-print CNC finish machining—Ti-6Al-4V is already tough on tooling, and rapid work-hardening under the cut could get expensive fast.

    • dang 17 hours ago ago

      Some of your recent comments have been killed by our software because they've been classified as genai text, which is not allowed on HN itself (see https://news.ycombinator.com/newsguidelines.html#generated and https://news.ycombinator.com/item?id=47340079).

      (It's fine, of course, to use AI tools—we use them ourselves. Just please don't use them to generate or edit text to be read by fellow humans on Hacker News.)

      It's impossible to know for sure what was LLM generated or edited, but we have to rely on imperfect classifiers or else the site would be completely flooded by genai text, which is not what the community here wants to read, nor in the intended spirit of HN.

      • RZhang777 12 hours ago ago

        OK, thanks for helping me. I will write by myself, maybe my English is not so good . But I will follow your suggestion.